Simulation of Hydrogen Diffusion in Fe and Fe-Based Alloys in Presence of Defects [14:10 - 14:30]
Authors: Daria Smirnova, Sergei Starikov
Understanding hydrogen embrittlement requires accounting for the interactions between hydrogen (H) and lattice defects. Such defects can act as hydrogen traps, significantly affecting its distribution and diffusion within a material. In this work, we employ classical atomistic simulations to investigate hydrogen behavior in Fe-based alloys containing a range of lattice imperfections, from vacancies to more complex defects such as grain boundaries (GBs) and dislocations. We present a modeling approach that enables consistent dynamic simulations of defects spanning multiple length scales within a single framework.
The simulations are based on a recently developed multipurpose interatomic potential for Fe-Cr-Ni-Ti-H system. The potential developed by the authors of current work was constructed in a form of an Angular-Dependent Potential (or ADP [1]). Such model ensures good applicability for simulating defects [2] and high computational efficiency. Examples demonstrating potential transferability across diverse compositions and defect configurations are also discussed.
Large-scale classical atomistic simulations were used as finite-temperature numerical experiments to determine the equilibrium distribution of hydrogen in Fe and Fe-Cr alloys containing crystal defects. Changes in hydrogen diffusion affected by vacancies, surfaces, and GBs were also studied over a wide temperature range. The simulation results show that the interaction between H and grain boundaries is highly sensitive to crystal structure and alloy composition. For example, in bcc-Fe, GBs may reduce H mobility relative to the bulk.
For bcc Fe–Cr alloys, hydrogen diffusion coefficients were calculated across a range of Cr concentrations. Increasing Cr content consistently reduces hydrogen diffusivity compared with pure bcc Fe. We further investigate how Cr influences hydrogen transport in bcc Fe grain boundaries. These calculations were performed using large GB models with Cr distributions equilibrated through combined MD/MC simulations. Using calculated hydrogen concentrations and diffusivities attributed to defects, we interpret existing experimental data on H permeation in Fe and Fe-based alloys.
References:
[1] Y. Mishin, M. Mehl, and D. Papaconstantopoulos. Acta mater. 2005, 53, 4029
[2] S. Starikov, D. Smirnova, T. Pradhan, I. Gordeev, R. Drautz, and M. Mrovec. Phys. Rev. Mater. 2022, 6, 043604